GH2696 一、化学成份(wt%):
C
Cr
Ni
Mo
Al
Ti
Fe
B
Si
Mn
P
S
≤0.1
10.0~12.5
21.0~25.0
1.0~1.6
≤0.8
2.6~3.2
余
≤0.02
≤0.6
≤0.01