Monel 502

Monel 502(NUS 05502)

1.Composition(wt%)

C

Ni

Cu

Fe

Al

Ti

Mn

Si

S

≤0.1

63.0-70.0

balance

≤2.0

2.5-3.5

≤0.5

≤1.5

≤0.5

≤0.01

2.Physical Properties

Density
 (g/cm3)

Melting point 
(°C )

8.03

1330

3.Mechanical Properties

Property

Tensile strength
(Annealing)MPa

Yield strength
(Annealing)MPa

Elongation
%

Poisson 
ratio

Elastic modulus
GPa

Monel 502

1158

1034

15

0.27-0.30

190-210

4.Applications

1.Fastener.
2.The shaft of the pump.
3.Transmission shaft.
4.Valve module.

 

 