Monel k-500 (UNS N05500)
1.Composition(wt%)
|
C
|
Ni
|
Fe
|
Cu
|
Ti
|
Al
|
Mn
|
S
|
Si
|
|
≤0.25
|
≥63.0
|
≤2.0
|
27.0-33.0
|
0.35-0.85
|
2.30-3.15
|
≤1.5
|
≤0.01
|
≤0.5
|
2.Physical Properties
|
Density
(g/cm3)
|
Melting point
(℃)
|
|
8.05
|
1288-1343
|
3.Mechanical Properties at room temperature
|
Tensile strength
MPa
|
0.2Yield strength
MPa
|
Elongation
%
|
|
1100
|
790
|
20
|
4.Characteristics
Monel K500 also name UNS N05500, the corrosion resistance is similar to Monel 400,
but the mechanical strength and hardness are much higher.
Good heat corrosion resistance and stable organization for long term use.
5.Applications
Mainly used in manufacturing turbine blade and gas turbine blade of aero-engine,
working temperature below 750℃; manufacturing fasteners and springs on the ships; pumps and valve
parts on the chemical equipments, starched blades of the papermaking, etc.
|