MonelR-405 (UNS N04405)
1.Composition(wt%)
|
C
|
Ni
|
Fe
|
Cu
|
Mn
|
S
|
Si
|
|
≤0.3
|
≥63.0
|
≤2.5
|
28.0-34.0
|
≤2.0
|
0.025-0.06
|
≤0.5
|
2.Physical Properties
|
Density
(g/cm3 )
|
Melting point
(℃)
|
Poisson ratio
|
Curie temperature
(℃)
|
|
8.8
|
1300-1350
|
0.32
|
21-49
|
3.Mechanical Properties at room temperature
|
Alloy and condition
|
Tensile strength
MPa
|
0.2Yield strength
MPa
|
Elongation
%
|
|
Monel R405
(hot working +annealing)
|
482-586
|
137-275
|
50-35
|
4.Characteristics
Since the elevated content of sulfur, having better machinability than Monel 400. And the corrosion resistance
and physical properties are similar to Monel 400, mechanical properties differ from Monel 400 slightly.
5.Applications
Monel R-405 is mainly used for manufacturing self-tapping screws.We do not recommended the Monel R-405 used in other areas.
|