MnCrWV
1.Composition(wt%):
|
C
|
Si
|
Mn
|
Cr
|
V
|
W
|
S
|
P
|
|
0.95-1.05
|
≤0.4
|
1.0-1.3
|
0.4-0.7
|
0.15-0.3
|
0.4-0.7
|
≤0.03
|
≤0.03
|
2.Properties:
|
Condition
|
Hardness
HRC
|
|
Standard hot treatment
|
60-62
|
3.Characteristics:
The deformation of steel belongs to low cold work die steel.
High carbon alloy tool steel.
Good comprehensive performance,
Pin salt can be graded hardened;
High strength, good machinability and hardenability,
Small heat treatment deformation.
4.Applications
Used in the manufacture of complex shape and load the molding parts, injection mould, etc.;
Requirements of making the commutability CrWMn deformation of small, complex shape of blanking
die light load, light load tensile, bending, flanging die, etc. |