Nimonic PE16

1.Composition(wt%)

C

Cr

Ni+Co

Fe

Mo

Cu

Al

Ti

Co

0.04-0.08

15.5-17.5

42.0-45.0

balance

2.8-3.8

≦0.5

1.1-1.3

1.1-1.3

≦2.0

Zr

B

Mn

Si

S

Pb

Ag

Bi

-

0.02-0.04

≦0.005

≦0.2

≦0.5

≦0.015

≦0.0015

≦0.0005

≦0.0001

-

2.Physical Properties

Density
(g/cm3

Melting point
(℃)

Specific heat capacity
(J/kg·℃)

Thermal conductivity
(W/m·°C)

Electric resistivity
(Ω·cm)

Thermal expansion coefficient
(20-100℃)/K

8.00

1310-1355

544

11.72

110×10E-6

13.8×10E-6

3.Mechanical Properties

1. Instantaneous rupture properties(bar, typical hot treatment)

Test temperature

Tensile strength
MPa

Yield strength
(0.2yield point)MPa

Elongation
%

Shrinkage of area
%

Kinetic Youngs modulus
GPa

20

830

450

29

55

192

300

770

380

31

54

180

600

680

410

30

51

161

900

140

100

74

96

134

1000

80

50

>100

98

122

2.High temperature endurance properties(bar,typical hit treatment)

Test temperature

Test time
h

Burst pressure
MPa

Elongation
%

650

1000

363

13-20

700

1000

255

21-28

750

1000

155

13-27

4.Applications

1.Parts used in nuclear reactors.
2.Used in gas turbine components.         

 