Instantaneous rupture properties(bar,typical hot treatment)
Test temperature
℃
Tensile strength
MPa
Yield strength
(0.2yield point)MPa
Elongation
%
Shrinkage of area
%
Kinetic Young’s modulus
GPa
20
1237
837
27
35
216
300
1175
787
26
32
200
600
1150
780
25
33
182
900
725
425
13
17
156
1000
375
112
27
19.5
141
4.Applications
Used for high temperature gas turbine components.