Nimonic 86
1.Composition(wt%) :
|
Ni
|
Ce
|
Cr
|
Mg
|
Mo
|
C
|
|
balance
|
0.03
|
25.0
|
0.015
|
10.0
|
0.05
|
2.Physical properties:
3.Mechanical Properties:
|
Properties at room temperature
|
Nimonic 86
|
|
Tensile strength(annealing)
(MPa)
|
825
|
|
Yield strength(annealing)
(MPa)
|
410
|
|
Elongation at break
(%)
|
42
|
|
Elastic modulus
(GPa)
|
210
|
4.Processing Technology:
1. Machinability
Can be used in the iron alloy in the traditional processing methods. This alloy will become hard when it works,
and shows a higher strength in the process of machining.
2. Weld
Welding by using the common techniques , using a matching filler metal.
3. Cold Working
The alloy can be hardened by cold work.
4. Annealing
Solution annealing.
5.Characteristics and applications:
Nickel - chromium - molybdenum alloy.
Good weldability , workability, ductility and creep.
Excellent oxidation resistance at high temperature.
6.Applications
1.Gas turbine engineering.
2.Industrial furnace.
3.The combustion chamber.
|