Nimonic-75 (UNS N06075、W.Nr.2.4951)
1.Composition(wt%) :
|
C
|
Cr
|
Ni
|
Fe
|
Cu
|
Ti
|
Mn
|
Si
|
|
0.08-0.15
|
18.0-21.0
|
balance
|
≤ 5.0
|
<0.5
|
0.2-0.6
|
≤ 1.0
|
≤ 1.0
|
2.Physical properties:
3.Mechanical Properties :
|
Properties at room temperature
|
Nimonic-75
|
|
Tensile strength(annealing)
(MPa)
|
750
|
|
Yield strength(annealing)
(MPa)
|
275
|
|
Elongation at break
%
|
42
|
|
Elastic modulus
(GPa)
|
206
|
4.Characteristics and Applications:
Good mechanical property and resistance to oxidation at high temperature.
Can be applied in the following aspects:
1.Aerospace fasteners,
2.Gas turbine engineering,
3. Industrial furnace structure,
4. Heat treatment equipment,
5. Nuclear engineering.
|