Nimonic 80A (UNS N07080/W. Nr. 2.4952)
1.Composition(wt%) :
|
C
|
Cr
|
Ni
|
Al
|
Ti
|
Fe
|
B
|
|
≤0.1
|
18.0-21.0
|
balance
|
1.0-1.8
|
1.8-2.7
|
≤3.0
|
≤0.008
|
|
Zr
|
Co
|
Mn
|
Si
|
P
|
S
|
Cu
|
|
≤0.15
|
≤2.0
|
≤1.0
|
≤1.0
|
≤0.02
|
≤0.015
|
≤0.2
|
2.Physical Properties:
|
Density
( g/cm3)
|
Melting point
(℃)
|
|
8.19
|
1320-1365
|
3.Mechanical Properties at room temperature:
|
Condition
|
Tensile strength
(MPa)
|
Yield strength
(MPa)
|
Elongation
%
|
|
Nimonic 80A
|
930
|
620
|
20
|
4.Characteristics:
Precipitation hardening alloys, high temperature ( up to 815 ° C) for excellent properties.
5.Applications:
Diesel engine exhaust valve of Vessels, tanks mainly made from Nimonic 80 a forging. High heat resistance,
high strength at high temperature, large deformation resistance, increased the difficulty of the forging. Suitable for
manufacturing bolt, exhaust valve of the combustion chamber.
|