Incoloy 832
1.Chemical Properties(wt%)
| Ni |
Cr |
Mo |
Fe |
Al |
Mn |
Ti |
Cu |
Si |
C |
S |
| 8.75-15.5 |
19.5-21.0 |
0.4 |
Balance |
0.15 |
0.4 |
0.4 |
≤0.75 |
0.7 |
≤0.05 |
≤0.005 |
2.Physical Properties
3.Mechanical Properties at room temperature
| Tensile strength |
Yield strength |
Elongation |
hardness
|
| MPa |
MPa |
% |
Rb |
| 346 |
762 |
37.5 |
82.3 |
4.Characteristics
The alloy exhibits excellent thermal stability and good resistance to hot salt corrosion, and to pitting.
It is readily formed and has excellent weldability.
5.Applications
Incoloy 832 is a low cost stainless steel developed specifically for domestic and industrial
sheathed heater applications.It is suitable for use on high output continuous strip welding
machines. |