Inconel686 (UNS N06686/W.Nr. 2.4606)
1.Chemical Composition(wt%)
| Cr |
Mo |
W |
Ti |
Fe |
C |
Mg |
S |
Si |
P |
Ni |
| 19.0-23.0 |
15.0-17.0 |
3.0-4.4 |
0.02-0.25 |
≤2.0 |
≤0.01 |
≤0.75 |
≤0.02 |
≤0.08 |
≤0.04 |
balance |
2.Physical Properties
density
(g/cm3) |
Melting range
(°C) |
electrical resistivity
(Ω*m) |
permeability
(15.9 kA/m) |
| 8.73 |
1338-1380 |
1.237 |
1.0001 |
3.Mechanical Properties at room temperature
| Condition |
tensile strength
(MPa) |
yield strength (MPa) |
Elongaion % |
| bars |
810 |
359 |
56 |
4.Characteristics
1.Good resistance in reducing conditions;
2.Good resistance to oxidizing media;
3.Resistance to general, pitting and crevice corrosion increases.
5.Applications
ggressive media in chemical processing, pollution control, pulp and paper manufacture, and waste
management applications. |