Inconel 603XL:
1.Composition(wt%)
|
C
|
Cr
|
Ni
|
Mo
|
Mn
|
Al
|
Ti
|
N
|
Si
|
rare earth
|
|
≤0.3
|
15-23
|
balance
|
≤4.0
|
≤0.3
|
≤0.5
|
≤0.5
|
0.02-0.07
|
≤2.0
|
≤0.1
|
2.Physical Properties
|
density
(g/cm3 )
|
melting point (℃)
|
specific heat capacity
(J/kg*℃ )
|
electrical resistivity (Ω*m)
|
|
8.54
|
1380-1400
|
439
|
1.16
|
3.Mechanical properties
Tensile properties at room temperature
|
tensile strenth (MPa)
|
yiels strength (MPa)
|
elongation %
|
|
790
|
410
|
50
|
4.Characteristics
Inconel 603XL with the addition of silicon, molybdenum and rare earth elements makes resistance to
high temperature oxidation and nitridation. The alloy has high mechanical strength and is readily
formed, machined and welded.
5.Applications
Furnace mesh belts utilized in the powder metal sintering industry and other thermal processing
applications |