Inconel617 (N06617)
1.Composition(wt%)
| C |
Cr
|
Ni
|
Fe
|
Mn
|
Si
|
Cu |
|
0.05-0.15
|
20.0-24.0
|
≥44.5
|
≤3.0
|
≤1.0
|
≤1.0
|
≤0.5 |
|
Mo
|
Co
|
Al
|
Ti
|
B
|
S
|
|
|
8.0-10.0
|
10.0-15.0
|
0.8-1.5
|
≤0.6
|
≤0.006
|
≤0.015
|
|
3.Mechanical Properties at room temperature
|
Condition
|
Tensile strength
MPa
|
Yield strength
MPa
|
Elongation
%
|
|
Solution treatment
|
680
|
300
|
30
|
4.Characteristics
Alloy in the field of hot corrosion environment such as sulfide, especially in the environment up to 1100 ℃
circulating oxidation and carbonization , has excellent corrosion resistance .
The corrosion resistance combined with excellent mechanical properties, makes it particularly suitable for
high temperature field, good transient and long term mechanical properties until the 1100 ℃.
|